Achieving 96-Hour Salt Spray Resistance for Aerospace Pins: SPierson's Proven Solution

Jun 04, 2025 Leave a message

 

Introduction:

In aerospace connector pin manufacturing (as shown in Figure 1), meeting stringent 96-hour salt spray test requirements presents a significant technical challenge. While most industry standards only require 48-72 hours of resistance, SPierson has developed a reliable dual-plating process that consistently achieves the demanding 96-hour standard.

The Challenge:

• Standard silver plating typically fails at 48-72 hours in salt spray testing

• Aerospace applications demand superior corrosion resistance

• Traditional methods cannot guarantee consistent 96-hour performance

SPierson's Innovative Solution:

Our proven two-step plating process:

1. Base Layer - Precision Nickel Plating:

- Creates a corrosion-resistant foundation

- Thickness controlled to 5-8μm

- Provides excellent adhesion for silver layer

2. Top Layer - High-Purity Silver Plating:

- 99.9% pure silver deposition

- Optimal thickness of 3-5μm

- Maintains superior electrical conductivity

Technical Advantages:

✓ Consistent 96+ hour salt spray performance

✓ Excellent wear resistance

✓ Maintains low contact resistance (<5mΩ)

✓ No peeling or blistering after testing

Process Validation:

- Tested per ASTM B117 standard

- 100% batch testing implementation

- Third-party verification available

info-1276-1276